SelectAlloy 317L-AP BF

Stainless Steel / Flux Cored / Gas Shielded


Features

  • Low C, < 0.04 wt%, minimizes carbide precipitation (sensitization) which makes the weld metal more resistant to intergranular corrosion.
  • The addition of Mo improves resistance to pitting and crevice corrosion compared to type 308 stainless steel with increased resistance compared to type 316 due to the nominal ~1 % increase (Mo).
  • Designed for welding in all positions where well washed beads can be achieved with minimal weaving in both 100% CO₂ or 75-80% Ar/balance CO₂ shielding gas
  • Smooth arc transfer produces minimal spatter.
  • Applications for this alloy type include welding components of similar composition or multilayer classing applications in severely corrosive environments, where crevice and pitting corrosion are of concern.

Standard Diameters

in (mm)
  • 0.035 (0.9)
  • 0.045 (1.2)
  • 1/16 (1.6)

Welding Positions

All Positions

Shielding

  • 75-80% Ar + Balance CO₂
  • 100% CO₂
    Flow Rate: 40 – 50 CFM

Polarity

Direct Current Electrode Positive (DCEP)

Conformances

  • ASME SFA 5.22
    • E317LT1-1
    • E317LT1-4
  • AWS A5.22
    • E317LT1-1
    • E317LT1-4
  • TYPICAL WELD DEPOSIT CHEMISTRY (WT%)
    Shielding Gas C Cr Cu Mn Mo Ni P S Si WRC-1992 Ferrite
    100% CO₂ 0.03 19.30 0.18 0.83 3.45 12.30 0.02 0.01 0.75 12
    75% Ar/25% CO₂ 0.03 19.40 0.17 0.87 3.46 12.40 0.02 0.01 0.81 13
    Bismuth is not intentionally added and is not known to be at levels greater than 0.002 wt%

    Packaging (lbs (kg))

    33 (15) Spools, 60 (27.2) Coils, 500 (226.8) Round Drum, 800 (362.9) Hex Drum, 900 (408.2) Hex Drum

    *Some packaging options may not be available depending on diameter and product. Special package options may be available upon request.