Select Ni4S

Low Alloy / Submerged Arc / Flux Shielded


Features

  • Contains additions of nickel and molybdenum to produce good low temperature toughness while maintaining a tensile strength that withstands heat treatment.
  • Better control of bead penetration than solid wire
  • Higher deposition rates than solid wire when run at the same current level
  • Exhibits a broader and shallower bead profile than solid wire – reducing the tendency for burn through
  • Capable of running directly over root passes with proper procedure – eliminating requirement for a hot pass
  • Easy slag removal – reduces post weld clean up time
  • Typical applications include pressure vessels, offshore oil equipment, bridges, and other structural applications
  • Arcflux BF-10MW helps to maximize the impact properties and is the recommended flux. Other basic fluxes can be used as well.

Standard Diameters

in (mm)
  • 5/32 (4.0)

Welding Positions

Flat and Horizontal

Shielding

  • ARCFLUX BF-10MW

    Polarity

    Direct Current Electrode Positive (DCEP)

    Conformances

  • AWS A5.23
    • F8A8-ECNi4-Ni4 (ARCFLUX BF-10 MW)
    • F9A8-ECNi4-Ni4
    • F9P6-ECNi4-Ni4
  • TYPICAL WELD DEPOSIT CHEMISTRY (WT%)
    Flux C Cu Mn Mo Ni P S Si
    ARCFLUX BF-10 MW 0.06 0.05 1.48 0.26 1.83 0.020 0.010 0.46
    Typical Mechanical Properties
    Flux Tensile Strength
    ksi (MPa)
    Yield Strength
    ksi (MPa)
    Elongation
    (%)
    WeldCondition PWHTTemp Charpy V-Notch
    -60 °F ft⋅lb (-51 °C J)
    Charpy V-Notch
    -80 °F ft⋅lb (-62 °C J)
    ARCFLUX BF-10 MW 102 (703) 91 (627) 26 As-Welded 43 (58) 32 (43)
    ARCFLUX BF-10 MW 99 (683) 87 (597) 26 PWHT 1150°F for 1 hr 26 (35)

    Packaging (lbs (kg))

    33 (15) Spools, 60 (27.2) Coils, 500 (226.8) Round Drum, 800 (362.9) Hex Drum, 900 (408.2) Hex Drum

    *Some packaging options may not be available depending on diameter and product. Special package options may be available upon request.