Select 410C

Stainless Steel / Metal Cored / Gas Shielded


Features

  • Requires preheat and postheat treatments to achieve satisfactory ductility for most applications.
  • Metal cored construction inherently provides better welding performance compared to solid wires.
  • Postweld heat treatment > 1150ºF may result in rehardening due to untempered martensite after cooling to room temperature.
  • Used for welding components of similar compositions or for the surfacing of carbon steels to resist corrosion, erosion, or abrasion, which can occur in valve seats and other valve parts.

Standard Diameters

in (mm)
  • 0.045 (1.2)
  • 1/16 (1.6)

Welding Positions

Flat and Horizontal

Shielding

  • Ar + 0.5-5% CO₂
  • Ar + 0.5-3% O₂
    Flow Rate: 40 – 50 CFM

Polarity

Direct Current Electrode Positive (DCEP)

Conformances

  • ASME SFA 5.22
    • EC410
  • AWS A5.22
    • EC410
  • TYPICAL WELD DEPOSIT CHEMISTRY (WT%)
    Shielding Gas C Cr Cu Mn Mo Ni P S Si
    Argon 0.07 12.9 0.02 0.50 <0.01 0.35 0.008 0.007 0.40

    Packaging (lbs (kg))

    33 (15) Spools, 60 (27.2) Coils, 500 (226.8) Round Drum, 800 (362.9) Hex Drum, 900 (408.2) Hex Drum

    *Some packaging options may not be available depending on diameter and product. Special package options may be available upon request.