Select 410NiMo-C

Stainless Steel / Metal Cored / Gas Shielded


Features

  • Contains less Cr and more Ni compared to standard 410 alloy to improve mechanical properties.
  • Metal cored construction inherently provides better welding performance compared to solid wires.
  • Postweld heat treatment > 1150ºF may result in rehardening due to untempered martensite after cooling to room temperature.
  • Used to weld CA6NM castings or similar materials, as well as light-gauge 405, 410, and 410S base metals.

Standard Diameters

in (mm)
  • 0.045 (1.2)
  • 1/16 (1.6)

Welding Positions

Flat and Horizontal

Shielding

  • Ar + 0.5-5% CO₂
  • Ar + 0.5-3% O₂
    Flow Rate: 40 – 50 CFM

Polarity

Direct Current Electrode Positive (DCEP)

Conformances

  • ASME SFA 5.22
    • EC410NiMo
  • AWS A5.22
    • EC410NiMo
  • TYPICAL WELD DEPOSIT CHEMISTRY (WT%)
    Shielding Gas C Cr Cu Mn Mo Ni P S Si
    Argon 0.01 12.00 0.05 0.50 0.50 4.30 0.009 0.015 0.35

    Packaging (lbs (kg))

    33 (15) Spools, 60 (27.2) Coils, 500 (226.8) Round Drum, 800 (362.9) Hex Drum, 900 (408.2) Hex Drum